Forging
Minimum setup
Forge (gas is easier than coal to start), anvil or a heavy 50+ kg rail section, 1–1.5 kg hammer, tongs, water bucket. Costs about one machine tool.
Temperatures by color
Dark cherry ~700°C, cherry ~850°C, orange ~1000–1100°C, yellow ~1200°C — forging range. Welding white ~1300°C+ — steel starts sparking and burning.
Basic operations
Drawing out, upsetting, punching, bending, twisting, tapering. Each is a separate hammer technique — practice on 8–10 mm rod.
Starter steel
Mild/low-carbon steel forgives mistakes, can't be hardened. 10–20 mm rod or square. Spring steel is stage two — needs heat treatment.
Safety
Cotton/leather, no synthetics (they melt). Always goggles. Scale flies on impact — no kids/pets nearby. Ventilation — forge CO is deadly.
First projects
Fire poker → hook → trivet → knife blank. The goal of the first 10 hours is feeling the metal, not a product.
Über Schmieden
Schmieden — Ausrüstung, Temperaturen nach Farbe, Grundtechniken, Sicherheit. Holz & Metall: Volumen, Profilgewicht, Elektroden, Zuschnitt, Kerndurchmesser. Nutzen Sie unsere Tools ohne Registrierung oder Softwareinstallation. Alle Berechnungen erfolgen in Ihrem Browser — Ihre Daten werden nie an einen Server gesendet.